Indium Blog

Peel Testing Adhesion of Metallization Paste

Category:
  • Indium Corporation
  • Solar

  • This is a short video demonstrating how easy it is for you to perform a quick peel test on a metallization and demonstrate its adhesion to a thin-film. substrate. 
     


    After your metallization sample is cured, simply apply 3M Scotch® packaging tape and flatten it onto your substrate with finger pressure. If any of the metallization peels off onto the tape, the sample fails the adhesion test.

    Authored by previous Indium Application Manager Jim Hisert