Is Lowest "Cost of Ownership" the Best Electronics Assembly Manufacturing Metric?
Folks, Let’s look in on Patty and her colleagues…... Sam Watkins, ACME New Hampshire site GM, had just finished meeting with his boss, A...
Folks, Let’s look in on Patty and her colleagues…... Sam Watkins, ACME New Hampshire site GM, had just finished meeting with his boss, A...
Readers have asked how to visually assess a tabbing ribbon interconnection after a bond test. This image is a cell that has been bond tested after sol...
With regard to soldering or wetting (coating) with indium, we are often asked to comment on the oxide formation of indium and how to remove it.......
We are often asked if it is possible to solder to stainless steel and, if so, what is the best procedure. As you may already know, stainless stee...
A customer raised an interesting question regarding the use of our indium plating......
We are frequently asked if it is possible to solder to aluminum. The answer is yes, if the following guidelines are followed: FLUXES: Becau...
Looking for tech papers that answer the most basic soldering questions? These rank among our most frequently downloaded: Five Solder Families and......
Folks, A reader writes: My company makes an electronic product that requires a 40 year shelf life. We assemble with tin-lead solder on FR-4 PWBs....
Here is a fairly common question as answered by our Tech Team: img height="225" align="right" width="300" title="In...
After the report by Isofoton regarding reliability testing of Bi-based alloys for tabbing ribbon, the world learned that Bi-based alloys could survive...
Here is a question that was posted and answered on our website back in 2006, I think it is still quite relevant: img align="right" alt="...