Head-in-pillow Defects Attract non-SMT Attention
What would bring a person from outside the SMT world to a website like Indium.com? Why would a marketing guru have interest in head-in-pillow de...
What would bring a person from outside the SMT world to a website like Indium.com? Why would a marketing guru have interest in head-in-pillow de...
The question often arises as to whether or not a water wash solder paste should be halogen-free. Since halogen-free is fundimentally an environm...
Folks, Recently someone asked me about reworking a SAC305 solder joint with a SnBi solder. The reason to consider SnBi was that the lower melting...
http://circuitsassembly.com/cms/component/content/article/199/7190-photovoltaics-in-ems-sector This article isn’t ‘hot off the press&rsquo...
This year we tried to plan something a little different for APEX. Instead of the normal booth,......
Images stolen (with permission) from the Power-Semiconductor Blog ......
http://circuitsassembly.com/cms/component/content/article/199/7190-photovoltaics-in-ems-sector This article isn’t ‘hot off the press&rsquo...
I assure you, the following is not some strange alien test of foreign materials. Even though it resembles a substance from the spaceship in E.T. ̵...