Soldering 80Au/20Sn with Specialized Fluxes & Formic Acid
Not all fluxes can handle the high processing temperature required for Au/Sn solder preforms....
Not all fluxes can handle the high processing temperature required for Au/Sn solder preforms....
Soldering without flux is generally regarded as difficult if not impossible. Yet a fluxless process is routinely done with 80Au/Sn ribbon and preforms...
Au/Sn is available in all the forms you would expect from conventional solder alloys. ...
Typically, applications that use gold-tin solders are structural or die-attach. Structural applications make use of the alloy’s high strength, w...
In my previous post we saw that 80Au/20Sn eutectic alloy performs as both a solder or a braze. This is due to its unique and valuable properties. Let&...
You may have heard the 80% gold 20% tin alloy referred to as a solder. Or, you may have heard it called a braze. I’m going to explain how both s...