Minimizing Graping
Folks, This post is an excerpt on graping, from Indium Corporation's The Printed Circuits Assemblers Guide to Solder Defects. Intr...
Folks, This post is an excerpt on graping, from Indium Corporation's The Printed Circuits Assemblers Guide to Solder Defects. Intr...
Folks, Chris Nash and I (supported by an army of Indium Corporation’s outstanding engineers) wrote a booklet on eliminating solder defects. The ...
The second stage of a reflow profile activates the flux in the solder paste and prepares the solder for reflow. This can be a critical stage...
En la actualidad en nuestros procesos de ensamble de SMT utilizamos aleaciones libres de plomo (Pb-Free), las cuales requieren temperaturas de proceso...