Soldering to Interesting Metal Surfaces
This study does not claim to be the first to experiment with soldering to ‘difficult’ metal surfaces, but it does include some surprises....
This study does not claim to be the first to experiment with soldering to ‘difficult’ metal surfaces, but it does include some surprises....
“Nines” refers to the purity of a material. For instance: 99.99% indium is often described as “Four Nines” and written as &ldq...