  • Stephen Brunhauer, Paul Hugh Emmett, and Edward Teller (founders of the BET theory) had a great idea almost 80 years ago: use the absorption of gas molecules to measure the surface area of a material. That same principle is still used today to categorize our indium, gallium, and germanium compounds. If you have a specific BET requirement, please contact us.

    Because we have a flexible manufacturing process, we provide more than just 'off-the-shelf' materials. We provide compounds that are tailored to your application.